Ok guys pretty much have completed the whole top cap with 1000 grit. I still have some frosted areas. Do I stay at it with the 1000 grit or move on? I am also having alot of trouble using the sanding block in the curved areas of the top cap. I read on here somewhere about using a sponge as a sanding block. What do you guys think? And thirdly I have some small spider cracks in the gelcoat. take a look at my photos and tell me what you think. Thanks
Frosting in a low area kind of a swell in the rail.
Frosting again in a contoured area.
Another view of the frosting. Even with the 1000 grit the boat is really starting to shine again!![]()
Spider cracks in the gel. They do look better (smaller) after the 1000 grit but I didn't want to over do it.
![]()